Tint Strength and Undertone: How to Select Pigment Carbon Black
How to read published tinting-strength minima on P1550 and C111, and how to judge undertone when the pigment TDS does not print one. No invented tint or undertone numbers.
Tint strength and undertone should be selected together, but they are not the same cell on a datasheet. On the DLcarb pigment TDS (printed 3 August 2025), furnace grade P1550 (printed as P1550B/P) publishes tinting strength ≥128%, and channel grade C111 (printed as C111B/P) publishes ≥130%. Those figures are specification minima, not a masstone ranking and not an undertone. Neither row publishes an undertone. Lock the visual target first, read the printed minima as floors, check the application-map columns that are actually marked, then compare candidates under a fixed film thickness, substrate and illuminant. Request the family TDS, the EU REACH SDS and a sample through Contact.
What the pigment TDS actually publishes
The values below are taken from the DLcarb pigment carbon black TDS (printed 3 August 2025). They are specification ranges, not results from a single production lot. This page does not invent a tighter tinting-strength number, a masstone jetness rank, or an undertone for either grade.
| Item | P1550 (furnace pigment) | C111 (channel pigment) |
|---|---|---|
| Form | B = beaded / granular; P = powder | B = beaded / granular; P = powder |
| Tinting strength | ≥128% | ≥130% |
| Oil absorption | 50±3 ml/100g | 100±10 ml/100g |
| Iodine / surface-area column | Iodine absorption 175±8 g/kg | Iodine-column figure 200±20 (specific surface area on channel grades; TDS footnote) |
| pH | 7~9 | 2.5±1 |
| Heating loss | ≤1.5% | ≤1.5% |
| Ash | ≤0.5% | ≤0.5% |
| 45 μm sieve residue | ≤50 ppm | ≤50 ppm |
| Undertone | Not published | Not published |
| Checked application-map columns | Plastics and plastic goods, water-based systems, masterbatch, sponge, sealants and epoxy — not solvent-based or powder-coating columns | Water-based, solvent-based and powder coatings — not plastics or masterbatch |
The two tinting-strength cells are close, and both are minima. A two-point gap on a ≥ basis is not evidence that C111 will look stronger, blacker, or bluer in your system than P1550. Oil absorption, pH and process family are published differences that affect wetting and dispersion; they are not a substitute for a color trial.
How to select by tint strength and undertone
- Lock the visual goal before comparing grades. Write jetness, undertone preference and hiding as a measurable target — a reference panel, an instrument range, or an accepted standard — and fix film thickness, substrate and viewing illuminant.
- Read tinting strength as a published floor. Use the ≥128% and ≥130% cells as specification minima from the sheet, not as a promise of relative strength in the finished film or part.
- Do not assign an undertone from this table. Blue, red or brown undertone is not printed on either row. Judge undertone only after a trial in your resin system under the conditions locked above.
- Shortlist from the application map, not from the slightly higher minimum. Plastics and masterbatch coloration starts from the P1550 row that is actually marked for those columns; coatings and inks, including solvent-based and powder systems, start from the C111 row. Application detail is on pigment carbon black for plastics masterbatch and dispersion and jetness in coatings and inks.
- Trial in your own dispersion window. If aggregates are not opened, jetness and undertone will drift and the printed tinting-strength floor will not rescue the result.
Is C111 always stronger because its tinting-strength minimum is ≥130%?
No. Both published figures are specification minima, and they sit two points apart. This page does not treat ≥130% as a higher jetness or a stronger tint in use. What you see after dispersion is jetness, undertone, hiding and surface state — not the raw minimum on the sheet.
Does the TDS publish undertone for P1550 or C111?
No. Undertone is not a printed column on either row. This page does not invent a blue, red or brown undertone for either grade. Compare undertone in your system against a reference panel, at the same film thickness and illuminant, and record the accepted window in the RFQ.
Can I start a plastics color trial with C111 because its tinting-strength minimum is slightly higher?
Not according to the published application map. Plastics, plastic goods and masterbatch are marked on P1550 and are not marked on C111. C111 is the coatings conversation on this site — water-based, solvent-based and powder coatings. Do not override the map with a two-point difference in a minimum.
What should the RFQ include?
The host system (coatings, inks or plastics masterbatch), the visual target (jetness, undertone preference, hiding), the reference panel or method, film thickness and illuminant if already fixed, the sample size, and whether you need TDS, SDS and COA fields. WhatsApp and phone: +86 150-8314-1412. We do not list prices, MOQ or Incoterms on this page.
Request a sample or quote · Sample & export · SDS, specs and export documents
Last updated: November, 2026