Acetylene Black vs Furnace Conductive Carbon Black

Acetylene black vs furnace conductive carbon black, compared with a published SP150 vs 80P table. Do not assign EHV shielding, water-blocking tape or plastics to SP150.

Acetylene black and furnace conductive carbon black both form electrical networks in compounds, but they are not drop-in substitutes. On the DLcarb conductive and antistatic TDS (printed 3 August 2025), SP-prefix names are acetylene blacks and numeric-prefix names are furnace conductive blacks. Acetylene grade SP150 publishes oil absorption 220~270 ml/100g, iodine absorption 85±10 g/kg and resistivity ≤0.25 Ω·cm. High-structure furnace grade 80P publishes oil absorption 440~530 ml/100g and iodine absorption 330±40 g/kg, with no published resistivity. Do not assign extra-high-voltage shielding, water-blocking tape, or conductive or antistatic plastics to SP150. Use the tables below, then request the family TDS, the EU REACH SDS and a sample through Contact.

How the TDS names the two processes

The family sheet is a process map as much as a grade list. SP-prefix grades, including SP150, are acetylene blacks. Numeric-prefix grades, including 80P, are furnace conductive blacks; the suffix P on 80P means powder. A shared CAS number (1333-86-4) does not make the two rows interchangeable. For a broader shortlist across the conductive family, start from the conductive carbon black selection guide. This page stays on the acetylene-versus-furnace comparison and uses the published SP150 and 80P rows as the worked example. It is not a pigment or high-purity selection page.

SP150 vs 80P: published figures

These values are taken from the DLcarb conductive and antistatic carbon black TDS (printed 3 August 2025). They are specification ranges, not results from a single production lot. Blank or “-” cells are left unpublished here as well.

ItemSP150 (acetylene)80P (high-structure furnace)
Process / formAcetylene (SP prefix)Furnace (numeric prefix); P = powder
Oil absorption220~270 ml/100g440~530 ml/100g
Iodine absorption85±10 g/kg330±40 g/kg
Heating loss≤0.50%≤1.5%
Ash content≤0.50%≤0.5%
pH8.5±17~9
Resistivity≤0.25 Ω·cmNot published (printed as “-”)
Iron (Fe)Not published (column blank)Not published (printed as “-”)

The published oil-absorption and iodine-absorption windows are substantially higher on 80P than on SP150. Heating loss is tighter on the SP150 row (≤0.50% versus ≤1.5%). Ash limits are published at the same numerical cap. The two pH windows overlap. This page does not invent a resistivity or Fe figure for 80P, and it does not invent an Fe limit for SP150.

What the application map marks — and what it does not

TDS columnSP15080P
Heat-tracing cablesMarkedNot marked
Extra-high-voltage cable shielding compoundsNot markedMarked
Cable water-blocking tapeNot markedMarked
Conductive and antistatic plasticsNot markedMarked
Conductive coatings, inks and paintsNot markedMarked
Conductive / antistatic silicone and rubberMarkedMarked
Supercapacitors; thermally conductive materialsMarkedMarked
Cathode and anode slurries; dry batteries; lead-acid batteries; fuel cellsMarkedNot marked
Lithium-ion, sodium-ion or solid-state batteriesNot markedNot marked

The map also marks SP150 for specialty ceramics, metallurgy, antistatic floor coatings, antistatic flooring materials, antistatic leather and antistatic coatings — but not for conductive coatings or conductive inks. 80P is additionally marked for antistatic floor coatings and flooring, conductive and antistatic leather, conductive and antistatic foam and sponge, aerospace seals, antistatic high-pressure hoses, and conductive rubber rollers. Cable-construction detail (heat-tracing versus extra-high-voltage shielding and water-blocking tape) is on conductive carbon black for wire and cable.

When is acetylene black the better starting point?

Start from the acetylene row when the brief matches a column that is actually marked on SP150 — heat-tracing cables, the slurry / dry-battery / lead-acid / fuel-cell group, or the shared silicone, rubber, supercapacitor and thermally conductive columns — and when a published resistivity limit of ≤0.25 Ω·cm is part of the file. That is not a reason to treat SP150 as a plastics, extra-high-voltage shielding or water-blocking grade.

Can SP150 be used in conductive or antistatic plastics?

Not according to the published application map. Those columns are not checked for SP150; they are checked for 80P. If the brief is a plastic or antistatic-plastic compound, start from the furnace row that is actually marked and say so in the inquiry. The same rule applies to extra-high-voltage cable shielding and cable water-blocking tape: those columns belong to 80P, not to SP150.

Does 80P publish a resistivity value?

No. The resistivity and iron columns on the 80P row are printed as “-”. This page does not fill either figure in. What 80P does publish is the high oil-absorption and iodine-absorption window above, plus heating loss ≤1.5%, ash ≤0.5% and pH 7~9. If you need a resistivity target, put the test method and the limit in the RFQ rather than reading one off this table.

What should the RFQ include?

The process you are comparing (acetylene, furnace or still open), the host polymer or system, the TDS column that matches the job, any resistivity or cleanliness target and its method, the sample size, and whether you need TDS, SDS and COA fields. WhatsApp and phone: +86 150-8314-1412. We do not list prices, MOQ or Incoterms on this page.

Request a sample or quote · Sample & export · SDS, specs and export documents